Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 2.38 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.38 GPa

@Strain 1.33 %,
Temperature 23.0 °C
345 ksi

@Strain 1.33 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal..
Secant Modulus 2.38 GPa

@Strain 3.70 %,
Temperature -40.0 °C
345 ksi

@Strain 3.70 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi..
Secant Modulus 2.38 GPa

@Strain 3.70 %,
Temperature -40.0 °C
345 ksi

@Strain 3.70 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
Secant Modulus 2.38 GPa

@Strain 2.10 %,
Temperature 23.0 °C
345 ksi

@Strain 2.10 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..