Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.34 GPa @Strain 0.500 %, Temperature 80.0 °C |
339 ksi @Strain 0.500 %, Temperature 176 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 2.34 GPa @Strain 3.70 %, Temperature 100 °C |
339 ksi @Strain 3.70 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |