Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.2825 GPa @Strain 2.40 %, Temperature 0.000 °C |
331.05 ksi @Strain 2.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |