Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.32 GPa @Strain 5.00 %, Temperature 23.0 °C |
191 ksi @Strain 5.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Secant Modulus | 1.32 GPa @Strain 4.40 %, Temperature 23.0 °C |
191 ksi @Strain 4.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Secant Modulus | 1.31 GPa @Strain 7.00 %, Temperature -40.0 °C |
191 ksi @Strain 7.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |