Secant Modulus 1.14 GPa

@Strain 2.40 %,
Temperature 80.0 °C
166 ksi

@Strain 2.40 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub..
Secant Modulus 1.14 GPa

@Strain 4.70 %,
Temperature 40.0 °C
166 ksi

@Strain 4.70 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Secant Modulus 1.14 GPa

@Strain 2.40 %,
Temperature 80.0 °C
166 ksi

@Strain 2.40 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing ..
Secant Modulus 1.14 GPa

@Strain 4.70 %,
Temperature 40.0 °C
166 ksi

@Strain 4.70 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..