Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.07 GPa @Strain 0.400 %, Temperature -40.0 °C |
1170 ksi @Strain 0.400 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |
|||
Secant Modulus | 8.05 GPa @Strain 0.210 %, Temperature 40.0 °C |
1170 ksi @Strain 0.210 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Secant Modulus | 8.07 GPa @Strain 0.180 %, Temperature 100 °C |
1170 ksi @Strain 0.180 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Secant Modulus | 8.07 GPa @Strain 2.22 %, Temperature -40.0 °C |
1170 ksi @Strain 2.22 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Secant Modulus | 8.09 GPa @Strain 1.90 %, Temperature 23.0 °C |
1170 ksi @Strain 1.90 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 8.09 GPa @Strain 1.65 %, Temperature -20.0 °C |
1170 ksi @Strain 1.65 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |