Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.7575 GPa @Strain 4.00 %, Temperature 80.0 °C |
109.9 ksi @Strain 4.00 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |