Secant Modulus 1.90 GPa

@Strain 4.96 %,
Temperature -40.0 °C
276 ksi

@Strain 4.96 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Secant Modulus 1.90 GPa

@Strain 4.96 %,
Temperature -40.0 °C
276 ksi

@Strain 4.96 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..