Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.89 GPa @Strain 1.13 %, Temperature -20.0 °C |
274 ksi @Strain 1.13 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Secant Modulus | 1.89 GPa @Strain 1.90 %, Temperature 40.0 °C |
274 ksi @Strain 1.90 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Secant Modulus | 1.89 GPa @Strain 4.60 %, Temperature -40.0 °C |
274 ksi @Strain 4.60 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring .. |
|||
Secant Modulus | 1.89 GPa @Strain 4.60 %, Temperature -40.0 °C |
274 ksi @Strain 4.60 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Secant Modulus | 1.89 GPa @Strain 0.560 %, Temperature 0.000 °C |
275 ksi @Strain 0.560 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |