Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.86 GPa @Strain 2.30 %, Temperature 80.0 °C |
270 ksi @Strain 2.30 %, Temperature 176 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Secant Modulus | 1.86 GPa @Strain 2.30 %, Temperature 80.0 °C |
269 ksi @Strain 2.30 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |