Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.2757 GPa @Strain 4.5039 %, Temperature 80.0 °C |
185.03 ksi @Strain 4.5039 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |