Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.921 GPa @Strain 2.80 %, Temperature 80.0 °C |
134 ksi @Strain 2.80 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |