Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.868 GPa @Strain 7.25 %, Temperature 100 °C |
126 ksi @Strain 7.25 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |