Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.575 GPa @Strain 4.80 %, Temperature 100 °C |
83.4 ksi @Strain 4.80 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Secant Modulus | 0.575 GPa @Strain 4.80 %, Temperature 100 °C |
83.4 ksi @Strain 4.80 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |