Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.524 GPa @Strain 5.00 %, Temperature 100 °C |
76.0 ksi @Strain 5.00 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Secant Modulus | 0.524 GPa @Strain 4.60 %, Temperature 100 °C |
76.0 ksi @Strain 4.60 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |