Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.402 GPa @Strain 4.10 %, Temperature 100 °C |
58.4 ksi @Strain 4.10 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Secant Modulus | 0.402 GPa @Strain 12.06 %, Temperature -20.0 °C |
58.3 ksi @Strain 12.06 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 0.402 GPa @Strain 0.910 %, Temperature 100 °C |
58.3 ksi @Strain 0.910 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |