Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.371 GPa @Strain 2.70 %, Temperature 100 °C |
53.9 ksi @Strain 2.70 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Secant Modulus | 0.371 GPa @Strain 25.9 %, Temperature -40.0 °C |
53.9 ksi @Strain 25.9 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Secant Modulus | 0.371 GPa @Strain 12.1 %, Temperature 0.000 °C |
53.8 ksi @Strain 12.1 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Secant Modulus | 0.371 GPa @Strain 25.9 %, Temperature -40.0 °C |
53.9 ksi @Strain 25.9 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |