Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.322 GPa @Strain 9.20 %, Temperature 80.0 °C |
46.7 ksi @Strain 9.20 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |