Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.306 GPa @Strain 10.8 %, Temperature 23.0 °C |
44.4 ksi @Strain 10.8 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |
|||
Secant Modulus | 0.306 GPa @Strain 12.9 %, Temperature 80.0 °C |
44.4 ksi @Strain 12.9 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |