Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.286 GPa @Strain 9.00 %, Temperature 100 °C |
41.4 ksi @Strain 9.00 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Secant Modulus | 0.286 GPa @Strain 9.00 %, Temperature 100 °C |
41.4 ksi @Strain 9.00 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |