Mechanical Properties Metric English Comments
Compressive Modulus 61.4 GPa

@Temperature 23.9 °C
8900 ksi

@Temperature 75.0 °F
Dry; Oven Cure 250°F, 90 min; ASTM D695
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..