Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 61.4 GPa @Temperature 23.9 °C |
8900 ksi @Temperature 75.0 °F |
Dry; Oven Cure 250°F, 90 min; ASTM D695 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |