Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.430 - 2.14 GPa | 62.4 - 311 ksi | Average value: 0.939 GPa Grade Count:8 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Compressive Modulus | 0.430 GPa | 62.4 ksi | ASTM D695 |
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |