Polymer Property : Compressive Modulus = 580 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..
Compressive Modulus 4.00 GPa
580 ksi
23°C; ASTM D695
UBE UPIMOL® S High Heat Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..
Compressive Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 1011 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)  (discontinued **)
Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P..
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho..
Compressive Modulus 4.00 GPa
580 ksi
Henkel Hysol EA 956 Paste Adhesive System
Very low viscosity, cures at room temperatureDesigned for wet lay-up repairApplications: Structural Repair Low Viscosity Wet Lay-Up