Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 36.0 - 119.3 GPa @Temperature -59.0 - 130 °C |
5220 - 17300 ksi @Temperature -74.2 - 266 °F |
Average value: 84.5 GPa Grade Count:11 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Compressive Modulus | 36.0 GPa @Temperature 130 °C |
5220 ksi @Temperature 266 °F |
90º, Wet; EN2850 Type B |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |