Polymer Property : Compressive Modulus = 50.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.350 GPa
50.8 ksi
average; perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..