Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.350 GPa | 50.8 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |