Polymer Property : Compressive Modulus = 5.24 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 5.24 GPa
760 ksi
ASTM D695
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Compressive Modulus 5.24 GPa
760 ksi
ASTM D695
Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..