Mechanical Properties Metric English Comments
Compressive Modulus 5.17 GPa
750 ksi
TM R050-38
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Compressive Modulus 5.17 GPa
750 ksi
TM R050-38
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..
Compressive Modulus 5.17 GPa
750 ksi
TriStar Ultracomp UC-200 Composite Bearing
Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m..
Compressive Modulus 5.17 GPa
750 ksi
Perpendicular to Laminate
TriStar Ultracomp UC-200 Composite Bearing
Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m..
Compressive Modulus 5.17 GPa
750 ksi
TriStar Ultracomp UC-300 Composite Bearing
Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family..
Compressive Modulus 5.17 GPa
750 ksi
Perpendicular to Laminate
TriStar Ultracomp UC-400 Composite Bearing
Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry ..
Compressive Modulus 5.17 GPa
750 ksi
Perpendicular to Laminate
TriStar Ultracomp UC-500 Composite Bearing
Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear li..