Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 4.48 GPa | 650 ksi | TM R050-38 |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Modulus | 4.48 GPa | 650 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 4.48 GPa | 650 ksi | Perpendicular to Laminate |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |
|||
Compressive Modulus | 4.48 GPa | 650 ksi | TM R050-38 |
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Modulus | 4.48 GPa | 650 ksi | TM R050-38 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |