Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.144 GPa | 311.0 ksi | Z direction; 0.05/min strain rate; ASTM D695 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |