Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.207 GPa | 30.0 ksi | TM R050-38 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Compressive Modulus | 0.207 GPa | 30.0 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/4-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 0.207 GPa | 30.0 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 3/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 0.207 GPa | 30.0 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |