Mechanical Properties Metric English Comments
Compressive Modulus 3.70 GPa
537 ksi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..