Polymer Property : Compressive Modulus = 2610 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 18.0 - 21.0 GPa
2610 - 3050 ksi
Average value: 19.8 GPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Compressive Modulus 18.0 GPa
2610 ksi
ASTM D-695
Glastic GLASTHERM HT220 Insulation Sheet
Glastherm Grade HT220 is a thermal insulation sheet that is a highly heat-resistant material that combines low thermal conductivity with very high compressive strength at molding temperature. It is..