Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.748 GPa | 253.5 ksi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |
|||
Compressive Modulus | 1.748 GPa @Temperature 23.0 °C |
253.5 ksi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |