Polymer Property : Compressive Modulus = 228 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.57 GPa
228 ksi
At 150°C; JIS K7208
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..