Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.57 GPa | 228 ksi | At 150°C; JIS K7208 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |