Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 11.2 GPa | 1630 ksi | ASTM D3410 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |