Polymer Property : Compressive Modulus = 11.2 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 11.2 GPa
1630 ksi
ASTM D3410
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply
Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal ..