Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 109.6 GPa @Temperature 24.0 °C |
15900 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel |