Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.87 - 1.97 GPa | 271 - 286 ksi | ASTM D695 |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |