Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.110 GPa | 16.0 ksi | Stabilized |
Hexcel® HexWeb® ACG®-1 Honeycomb Aluminum Commercial Grade HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. .. |
|||
Compressive Modulus | >= 0.110 GPa | >= 16.0 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Compressive Modulus | 0.110 GPa | 16.0 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Compressive Modulus | >= 0.110 GPa | >= 16.0 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Compressive Modulus | 0.110 GPa | 16.0 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |