Mechanical Properties Metric English Comments
Compressive Yield Strength 6.21 MPa

@Strain 1.00 %
901 psi

@Strain 1.00 %
ASTM D695
Saint-Gobain Fluoroloy® A09 High Performance Seal Material
Extremely tough, long-wearing material; Excellent in water and water-based fluids, particularly suitable for abrasive media; Long wear life under severe conditions; Limited heat and chemical resista..