Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 6.21 MPa @Strain 1.00 % |
901 psi @Strain 1.00 % |
ASTM D695 |
Saint-Gobain Fluoroloy® A09 High Performance Seal Material Extremely tough, long-wearing material; Excellent in water and water-based fluids, particularly suitable for abrasive media; Long wear life under severe conditions; Limited heat and chemical resista.. |
|||
Compressive Yield Strength | 6.21 MPa | 900 psi | Stabilized, typ |
Hexcel® HexWeb® HRP - 3/16 - 5.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Compressive Yield Strength | 6.21 MPa | 900 psi | |
Aptek DI-STRATE 95197 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Auto RadarInformation provided by Aptek Lab.. |