Polymer Property : Compressive Yield Strength = 894 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 894 MPa
130000 psi
Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; EFA TP-003
Hexcel® HexPly® 920CX-FM40J-6-42% 125°C Curing Epoxy Matrix
High modulus carbon, Unidirectional, 165 g/m2Information provided by HexCel