Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 896 MPa @Temperature 23.0 °C |
130000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 896 MPa @Temperature 23.0 °C |
130000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 896 MPa @Temperature 23.0 °C |
130000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 894 MPa | 130000 psi | Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; EFA TP-003 |
Hexcel® HexPly® 920CX-FM40J-6-42% 125°C Curing Epoxy Matrix High modulus carbon, Unidirectional, 165 g/m2Information provided by HexCel |