Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 540 MPa | 78300 psi | 0° |
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, E-glass Balanced fabric 390 g/m2 Information provided by HexCel |
|||
Compressive Yield Strength | 540 MPa | 78300 psi | 0º |
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 300 g/m2 Information provided by HexCel |