Polymer Property : Compressive Yield Strength = 73.08 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 73.08 MPa
10600 psi
Abatron AboCast 8-18/Abocure 8-18 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c..