Compressive Yield Strength 66.0 MPa
9570 psi
ASTM D695
Adell AD-10 Nylon 66, Ultra High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 66.0 MPa
9570 psi
ASTM D695
Adell AD-30 Nylon 66, Ultra High Impact
Data provided by Adell Plastics, Inc.