Polymer Property : Compressive Yield Strength = 58.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 58.1 MPa
8420 psi
ASTM D695
Devcon HVAC Repair (Special F) Epoxy
General Repair EpoxyComments: Aluminum-filled epoxy adhesive, conveniently packaged in two 6.5 oz. tubes. Bonds to aluminum and other metals, ceramics, wood, concrete or glass. Use as an adhesive ..